On 56 days of curing time, OP-10M shows a highly significant MCS compared with TP and DM, which refers to the possibility of preparing OP-AAS with high MCS, mitigating the alkaline activator's harmful effect, and using low energy.
← all excerpts
Utilization of optimized microwave sintering to produce safe and sustainable one-part alkali-activated materials.