The flexural strength of the samples showed an increasing trend from 3 to 14 days, and the maximum flexural strengths of A, B 3 , and D 3 at 14 days were 3.8 MPa, 4.5 MPa, and 4.3 MPa, respectively.
← all excerpts
Study on hydration mechanism and environmental safety of thermal activated red mud-based cementitious materials.