aeruginosa demonstrated an increasing trend of 0.074 mm a –1 , which was 2.96 times higher than that of the abiotic control. 3.3.
← all excerpts
Mechanism underlying the acceleration of pitting corrosion of B30 copper-nickel alloy by <i>Pseudomonas aeruginosa</i>.
2
—
—
The sentences
aeruginosa started to show a decreasing trend at 7 days.