It can be seen from Figure 1 a that with the gradual increase of 1250 mesh in CaCO 3 content, the tensile strength and elongation at the break of the films show a decreasing trend.
← all excerpts
Research on Properties of PBAT/CaCO<sub>3</sub> Composite Films Modified with Titanate Coupling Agent.