As shown in Figure 6 a′−c′, all values of μ ′, μ ′′, and magnetic loss tangent (Tan δ ε = μ ′′/ μ ′) for composites demonstrate an increasing trend with slight fluctuations around 1.0, 0.0, and 0.0, which is probably caused by stronger multiple natural resonances at higher frequency [ 45 ].
← all excerpts
Morphology and Microwave-Absorbing Performances of Rubber Blends with Multi-Walled Carbon Nanotubes and Molybdenum Disulfide.
2
—
—
The sentences
Similarly, ε ′′ values of all samples also exhibit a decreasing trend with a fluctuation around the 9.0 GHz range of 2–18 GHz, and this fluctuation is ascribed to the presence of multiple dielectric relaxation polarizations [ 44 ].