However, as the incubation time further prolonged to 49 days, the swelling volume of the LDCUs showed a decreasing trend, because the nitrogen concentration in the coating layer reduced after the osmotic pressure difference decreased [ 55 , 56 ].
← all excerpts
Green construction and release mechanism of lignin-based double-layer coated urea.