At the age of 7 days, it is evident that with the increase in fine sand content, the drying shrinkage of samples S1–S6 shows a decreasing trend.
← all excerpts
Study on Shrinkage in Alkali-Activated Slag-Fly Ash Cementitious Materials.
1
—
—
At the age of 7 days, it is evident that with the increase in fine sand content, the drying shrinkage of samples S1–S6 shows a decreasing trend.