Interestingly, at a higher regime of CNC content (1–4 wt %), the MOR of the composite exhibited an increasing trend and reached a maximum value of 8.56 MPa at 4 wt % of CNCs (35.4% increase as compared to the control).
← all excerpts
On the Roles of Cellulose Nanocrystals in Fiber Cement: Implications for Rheology, Hydration Kinetics, and Mechanical Properties.