After 56 days, the shrinkage deformations between the sea concrete (1.07 mm/m) and the control concrete (0.97 mm/m) had a fading character; - the combination effect of sea concrete as an SCHSC with textile reinforcement on the tensile strength (3.6 MPa) shows equal results to the control concrete (3.3 MPa) with a slightly increasing trend.
← all excerpts
Self-Compacting High-Strength Textile-Reinforced Concrete Using Sea Sand and Sea Water.