The variation in tensile strength was similar for different drawing rates: it exhibited an increasing trend followed by a plateau as the strain increased, reaching its peak at a strain of 0.6 in all cases (815.3 MPa, 839 MPa, and 828.85 MPa).
← all excerpts
Study on the Effect of Cold Deformation and Heat Treatment on the Properties of Cu-Ag Alloy Wire.