When the content of MSW-IBA ground ash is 30%, its compressive strengths at 1, 7, and 28 days are 1.4, 2.4, and 3.6 MPa, respectively; with the increase of the content of MSW-IBA ground ash, the compressive strength of PFSS at 1, 7, and 28 days showed a decreasing trend.
← all excerpts
Test study on mechanical properties of compound municipal solid waste incinerator bottom ash premixed fluidized solidified soil.