From Figure 9 b, it can be seen from the curve that the maximum elongation roughly shows a decreasing trend with increasing strain rate at the same temperature, but, at low temperatures 223.15 K and 343.15 K, the conditions do not strictly follow this law and exhibit a greater dispersion, showing similar change trend at the two temperatures.
← all excerpts
Study on Mechanical Properties and Failure Mechanisms of Highly Filled Hydroxy-Terminated Polybutadiene Propellant under Different Tensile Loading Conditions.