As shown in Figure 2 h, the results of degradation profiles displayed a decreasing trend of the relative weight, and the average weight loss of pure TCP and (1, 2, 4)WES-TCP scaffolds immersed in the Tris–HCl solution for 28 days was 10.31, 27.47, 30.67, and 34.46%, respectively.