Both values showed a decreasing trend from (51.39 ± 4.72) ns to (27.35 ± 1.16) ns for long-range diffusion and from (0.522 ± 0.018) ns to (0.303 ± 0.004) ns for short-range lithium jumps after annealing samples at 200 and 500 °C, respectively ( Figure S6 ).