As illustrated in Figure 3 a, there is an obvious trend observed in the magnetic moment of silicene: as the f laser decreases from 1316.8 THz to 13.2 THz, the magnetic moment of silicene exhibits a gradual increase, ranging from 0.12 μ B to 0.35 μ B .