Independent t -test showed a p -value of 0.001, revealing a statistically highly significant difference in mean resin tag length between the groups, which in turn signifies group II sealant (10.03 ± 1.00 μm) found to be superior to the group I sealant (7.46 ± 0.95 μm) ( Table 2 ).
← all excerpts
<i>In Vitro</i> Evaluation of Viscosity, Depth of Penetration, Microleakage, and Shear Bond Strength of Conventional and Hydrophilic Sealants.