Result Surface microhardness (SMH) value after pH cycling of GIC (45 ± 10.23) and SDF (47.76 ± 6.69) is statistically highly significant (<0.001) compared to the baseline SMH of both test groups.
← all excerpts
Comparative Evaluation of Effect of Silver Diamine Fluoride and Glass Ionomer Cement on Microhardness of Artificial Caries Lesion in Primary Teeth: An <i>In Vitro</i> Study.