The weight loss rate of TIG remelting and unremelted specimens exhibits the same trend, with an increasing trend in weight loss rate as the corrosion time prolongs.
← all excerpts
Effect of Tungsten Inert Gas Remelting on Microstructure and Corrosion Resistance of Q450NQR1 High-Strength Weathering Steel-Welded Joints.