As expected, an increasing trend in austenite vol.% was observed with increasing IAT from 680 °C to 740 °C.
← all excerpts
Process Maps for Predicting Austenite Fraction (vol.%) in Medium-Mn Third-Generation Advanced High-Strength Steels.
1
—
—
As expected, an increasing trend in austenite vol.% was observed with increasing IAT from 680 °C to 740 °C.