Although in the all BTAS glass ceramic samples the differences in the peak frequencies between the ‐Z′′ and M′′ versus frequency plots does not show an apparent trend, the mismatch of the peak frequency found in the BTAS‐3 glass ceramic is still the smallest, which indicates that the BTAS‐3 glass ceramic has the minimum dielectric mismatch.
← all excerpts
Boosting Energy Storage Performance of Glass Ceramics via Modulating Defect Formation During Crystallization.
1
—
—