The part density showed an increasing trend at the slower scan speed of 800 mm/s due to the longer consolidation time and increasing laser power.
← all excerpts
Surface Roughness of Interior Fine Flow Channels in Selective Laser Melted Ti-6Al-4V Alloy Components.
1
—
—