An increasing trend in strength is observed with the addition of CSW up to 4.5 kg/m 3 , which represents the optimal content for both w / b ratios.
← all excerpts
Enhancing Concrete Mechanical Properties through Basalt Fibers and Calcium Sulfate Whiskers: Optimizing Compressive Strength, Elasticity, and Pore Structure.