6 a,b, Ra exhibited a decreasing trend with the increase of n 2 as the spindle speeds n 1 gradually increased under A u = 10 μm, I = 3 A, and t = 80 min.
← all excerpts
Improvement of roughness in ultrasonic assisted magnetorheological finishing of small titanium alloy nuts by orthogonal test method.