Meanwhile, the SFE exhibited an increasing trend, measuring at 24.3 ± 1.46 mN/m, 24.8 ± 1.53 mN/m, 24.1 ± 0.62 mN/m and 23.9 ± 2.60 mN/m.
← all excerpts
In Situ Reduction of Silver Nanoparticles/Urushiol-Based Polybenzoxazine Composite Coatings with Enhanced Antimicrobial and Antifouling Performances.