With increased MgO particle content, the compression modulus displayed an increasing trend from SF scaffolds to SF-3nMgO scaffolds, relative to 58.75 ± 14.03 kPa for SF scaffolds, 109.25 ± 9.91 kPa for SF-1nMgO scaffolds and 245.66 ± 24.21 kPa for SF-3nMgO scaffolds.