An increasing trend is observed in the P.F. for both materials and at 800 K it becomes 3.7 × 10 11 W mK −2 s −1 for Cl-based material and 5 × 10 11 W mK −2 s −1 for Br-based material.
← all excerpts
Exploring half-metallic ferromagnetism and thermoelectric properties of Tl<sub>2</sub>WX<sub>6</sub> (X = Cl and Br) double perovskites.