This behavior is observed in the viscosity results shown in Figure 2 , where an increasing trend in viscosity against frequency is evident for PHBH at 180 and 200 °C.
← all excerpts
Tuning the Structure-Property Relationships in Binary and Ternary Blends of PLA/PBAT/PHBH.