The Effect of Interlayer Delay on the Heat Accumulation, Microstructures, and Properties in Laser Hot Wire Directed Energy Deposition of Ti-6Al-4V Single-Wall.

Materials (Basel) · 2024 · PMC11243745 · PMID 38998387

2
hedged sentences
closest p
boldest claim

The sentences

a decreasing trendno p-value reported
A decreasing trend of Al wt.% was recorded with an increase in the build height for the wall made without interlayer delay, as shown in Figure 7 a.

also in 47,180 other papers

an increasing trendno p-value reported
When lath thickness values were plotted as a function of build height up to 15 mm considering only the characteristic regions ( Figure 9 a), an increasing trend of lath thickness with increasing build height was observed for all three samples.

also in 63,971 other papers