Characterization of Melt-Spun Recycled PA 6 Polymer by Adding ZnO Nanoparticles during the Extrusion Process.

Polymers (Basel) · 2024 · PMC11244155 · PMID 39000738

1
hedged sentence
closest p
boldest claim

The sentences

a decreasing trendno p-value reported
The results of the thermal analysis show an increase in the glass transition temperature of the extruded material from 50.97 °C (raw polymer) to 51.40 °C to 57.98 °C (polymer modified with ZnO NPs) and an increase in the crystallization point from 148.19 °C to a temperature between 175.61 °C and 178.16 °C, while the molar enthalpy (ΔHm) shows a decreasing trend from 65.66 Jg −1 (raw polymer) to 48.23 Jg −1 (PA 6 2.0% ZnO).