The R value for Zn(002) exhibits an increasing trend, rising rapidly from 0.2 during the first deposition to 0.51 during the fifth deposition (4 cycles), and then stabilizing at ≈0.5 during cycles 4 to 19.
← all excerpts
Three-in-One Zinc Anodes Created by a Large-scale Two-Step Method Achieving Excellent Long-Term Cyclic Reversibility and Thin Electrode Integrity.