While the left-edge and right-edge flash areas increased with deposit height, as a percentage of the total area, they did not follow an obvious trend with increasing deposit height.
← all excerpts
Evolution of Material Properties and Residual Stress with Increasing Number of Passes in Aluminium Structure Printed via Additive Friction Stir Deposition.