However, when the sulfuric acid concentration is more than 55%, the extraction rates of Ti, Al, and Mg components show a decreasing trend.
← all excerpts
Synergistic Leaching of Titanium, Aluminum, and Magnesium Components during Dilute Acid Pressure Treatment of High-Titanium Blast Furnace Slag.