As the content of the BIPB and TAIC increased, a decreasing trend in the elongation at break was observed, alongside an increasing trend in modulus, as shown in Fig. 3b .
← all excerpts
Highly elastic relaxor ferroelectric <i>via</i> peroxide crosslinking.
1
—
—