In Group A specimens, the unit volume weight value decreased from 2156 to 2048 with a decreasing trend from the SCM1-0 set to the SCM6-40 set.
← all excerpts
Effect of curing conditions on cement based self-compacting mortar produced with mortar waste aggregate.
2
—
—
The sentences
The decreasing I0 value among SCM1-0, SCM2-5 and SCM3-10 sets follows an increasing trend towards SCM4-20, SCM5-30, and SCM6-40.