Additionally, the specimen exhibited an increasing trend in recovery stress during the cooling process, which is attributed to the increase in both elastic modulus and recovery stress caused by the thermally induced martensitic transformation during cooling [ 49 ].
← all excerpts
Mechanical and Fatigue Properties of Welded Fe-Mn-Si Shape Memory Alloys.
2
—
—
The sentences
On the other hand, the recovery stress of the SWN specimen showed a decreasing trend until it reached the maximum temperature at a heating temperature of more than 200 °C, as shown in Figure 14 b.