1e ) demonstrates that, at high potential (4.5–4.8 V), high valence Ni is reduced to a low valence state during the oxidation of PEO, although the Ni valence of the whole cathode particle showed an increasing trend (Fig. 1f ).
← all excerpts
Strong Lewis-acid coordinated PEO electrolyte achieves 4.8 V-class all-solid-state batteries over 580 Wh kg<sup>-1</sup>.