A highly significant difference was found between as-received thermal NiTi group (83.51 ± 6.49 N/mm) and samples recycled by dry heat (53.73 ± 4.72 N/mm), autoclave (45.38 ± 4.37 N/mm), and cold sterilization (48.44 ± 3.12 N/mm) at 0.5 mm of deflection.
← all excerpts
The effect of different clinical recycling methods on load deflection properties of super-elastic and thermal nickel-titanium orthodontic arch wires: A comparative assessment.