As shown in Figure 15 , 3424 cm −1 is the peak associated with carbamate, and the overall peak area at this position shows a decreasing trend, indicating that the structure of the polyurethane hardness part has been damaged.
← all excerpts
Durability Investigation of Ultra-Thin Polyurethane Wearing Course for Asphalt Pavement.