The peak deviator stress shows a decreasing trend with decreasing freezing temperature, particularly between −5 °C and −10 °C, and then gradually stabilizes.
← all excerpts
Mechanical Properties and Damage Constitutive Model of Saturated Sandstone Under Freeze-Thaw Action.