Degradation of the Zn alloy in Hank’s solution exhibited a decreasing trend with prolonged immersion, eventually stabilizing at 16 μm/year.
← all excerpts
Biodegradable zinc alloys with high strength and suitable mechanical integrity as bone repair metals.