Barely Significant
← all excerpts

Comparative analysis of bulk ceramics and thick film coatings for optimized energy storage technologies.

Sci Rep · 2024 · PMC11686106 · PMID 39738475

1
hedged sentence
closest p
boldest claim

The sentences

an increasing trendno p-value reported
Figure 3 c shows coating thickness as a function of voltages (225–275 V) and time (30–180 s) with linear fitted lines indicating an increasing trend.

also in 63,971 other papers