However, the monoclinic phase fraction was lowest at 2 mol% CeO 2 doping, and it showed an increasing trend as the doping concentration increased beyond that.
← all excerpts
Phase Transformation Behavior, Mechanical Properties Under Thermal Stress, and Slag-Induced Erosion of 2-4 mol% CeO<sub>2</sub>-Doped CaO-Stabilized Zirconia.