Table 1 presents the carbon residue rate after thermal decomposition, revealing an increasing trend in carbon residue content with the addition of flame-retardant treatments: A0 < A1 < A2 < A6.
← all excerpts
Development of a Fire-Retardant and Sound-Insulating Composite Functional Sealant.