SD-mannitol formulations demonstrated an increasing trend of yield from F1 through to F2 and F3 (38.17 ± 2.61, 60.73 ± 4.12, and 63.64 ± 2.35%, respectively); this corresponded to increases in inlet temperature from 80 to 120 to 160 °C.
← all excerpts
Investigation of Spray Drying Parameters to Formulate Novel Spray-Dried Proliposome Powder Formulations Followed by Their Aerosolization Performance.