The tear strength exhibited an increasing trend with OPTB loading up to 70 phr ( Figure 8 b).
← all excerpts
Evaluating Oil Palm Trunk Biochar and Palm Oil as Environmentally Friendly Sustainable Additives in Green Natural Rubber Composites.