The elongation at break of the vulcanizates with applied ethylene glycol and both glycerols showed an increasing trend and reached a maximum at 20 phr of plasticizers.
← all excerpts
Influence of Plasticizers on Cross-Linking Process, Morphology, and Properties of Lignosulfonate-Filled Rubber Compounds.
2
—
—
The sentences
The M300 showed a decreasing trend with an increasing amount of plasticizer, again following the trend of the cross-link density.