The addition of CTAB reduced the surface free energy of the solution, thus speeding up the nucleation rate, so the average size of the α-Al 2 O 3 precursor presented a decreasing trend.
← all excerpts
Fabrication of Network Spherical α-Al<sub>2</sub>O<sub>3</sub> and Its Application on the Separator of Lithium-Ion Batteries.