The crystallinity of the matrix exhibited an increasing trend from approximately 39% for neat PCL to 43% for the 5 wt.% DPMF biocomposites.
← all excerpts
Improved Mechanical and Thermal Properties of Date Palm Microfiber-Reinforced PCL Biocomposites for Rigid Packaging.