However, from the DSC thermograms in Figure 5 , it can still be observed that there is an increasing trend in the baseline from 270 to 350 °C after complete polymerization, which has been confirmed by FTIR spectroscopy.
← all excerpts
Exploration of Poorly Recognized Advantages of Supply Chain Sustainable, Various Aliphatic Multiamine-Based Polybenzoxazines.