[ 10 ] In Figure 5d , composition profiles calculated along cylindrical regions of interest (Φ15 nm) at 5 nm intervals reveal a widening of the low Zn composition region, with a width of ≈50 nm The Zn–Zn RDF0 data from regions situated 70–120 nm from the grain boundary are plotted in Figure 5e , revealing an increasing trend in RDF0 from as‐quenched state to 1 week.
← all excerpts
Using Spinodal Decomposition to Investigate Diffusion Enhancement and Vacancy Population.